Дом блог

YLD-S0102 DVE-3: Low Volatility Vinyl Ether for UV Curing Formulas

архивы
Теги
YLD-S0102 DVE-3: Low Volatility Vinyl Ether for UV Curing Formulas
July 23, 2026

Product Name: Triethylene Glycol Divinyl Ether

Product Code: YLD-S0102

CAS No.: 765-12-8

Product Category: Active Diluent / Di-functional Vinyl Ether Monomer

 

1. Product Information

Item

Information

Product Name

Triethylene Glycol Divinyl Ether

Other Names

DVE-3;tri(ethylene glycol) divinyl ether;DIVINYL TRIETHYLENE GLYCOL DIETHER

Product Code

YLD-S0102

CAS No.

765-12-8

Molecular Formula

C10H18O4

Molecular Weight

202.25 g/mol

Category

Low-volatility, low-viscosity di-functional vinyl ether monomer

 

2. Product Description

YLD-S0102, Triethylene glycol divinyl ether, is a colorless to pale yellow liquid with low volatility. It is soluble in water and common organic solvents.

With vinyl ether reactivity and flexible triethylene glycol ether chains, it can be used in light-curing, UV-curing adhesives, sealants, resins, coatings, spray paints and adhesive systems. As a reactive diluent or crosslinking monomer, it helps adjust formulation viscosity and participate in curing or crosslinking reactions.

 

3. Structure Features and Key Advantages

1. Di-functional vinyl ether structure

YLD-S0102 contains two vinyl ether reactive groups and can participate in crosslinking reactions in relevant curing systems.

2. Low volatility and low viscosity

The product has low volatility and is suitable for formulation systems requiring processing stability. It can also help reduce system viscosity and improve mixing, flow and processing operation.

3. Good system compatibility

The flexible triethylene glycol ether chains support flexibility and compatibility in material systems. The product is soluble in water and common organic solvents, which makes it suitable for formulation development in resin, coating, sealant and adhesive systems.

 

4. Typical Properties

Item

Typical Value

Appearance

Colorless or light yellow liquid

DVE-3 Content, %

≥98.0

Boiling Point, °C

120-126

Density, g/mL @25 °C

0.99

Moisture Content, %

≤0.20

 

Note: The above data are from Typical Properties in the company TDS. Final delivery specifications shall be subject to the company TDS / COA.

 

5. Features

Feature

Description

Low volatility

Helps reduce volatilization loss during use and is suitable for systems requiring processing stability.

Reactive dilution

Can reduce system viscosity while participating in the curing process, helping reduce the performance impact of inert diluents.

Crosslinking ability

The di-functional vinyl ether structure can participate in crosslinked network formation and is suitable for crosslinking agent and reactive monomer applications.

System compatibility

Soluble in water and common organic solvents, supporting formulation adjustment in coatings, adhesives, sealants and resin systems.

 

6. Applications

1. Light-curing and UV-curing systems

YLD-S0102 can be used as a reactive diluent monomer in light-curing or UV-curing adhesives, sealants and coating systems to adjust formulation viscosity and participate in curing or crosslinking reactions.

2. Cross-linking agent

With its di-functional vinyl ether structure, the product can be used as a crosslinking monomer in relevant polymer systems. The TDS mentions its use as a crosslinker in the production of polyacrylate ion exchange resins.

3. Sulfur based sealant

YLD-S0102 can be used as a component in sulfur-based sealant compounds. Dosage and final performance should be confirmed by formulation testing.

4. Industrial systems such as coatings, resins and adhesives

Due to its low volatility and solubility in water and common organic solvents, it can also be used in fibers, resins, coatings, spray paints and adhesives, mainly as a solvent, reactive diluent or modifier.

 

7. Storage, Packaging & Safety

Item

Information

Packaging

Drums;IBC tanks

Storage temperature

5-30°C

Storage & Handling

Avoid direct sunlight and place in a cool and dry place. Avoid strong oxidants and acids.

Storage Life

12 months from the date of manufacture in the original packing in ambient temperatures.

Safety

All safety information is provided in the Material Safety Data Sheet.

 

оставить сообщение

оставить сообщение
Если вы заинтересованы в нашей продукции и хотите узнать более подробную информацию, пожалуйста, оставьте сообщение здесь, мы ответим вам, как только сможем.
Представлять на рассмотрение

Дом

Продукты

WhatsApp

Связаться с нами